I use a 3M Perfect It IIproduct 39002 Fine Cut and 39003 Micro-Finish compound specifically used for plexiglas.

My dad retired from Tinker Air Force Base and this iswhat the Airforce uses on aircraft windshields.

It works very well onthe windshield of my '94 1500 SE. I've used it on 5 Goldwings.
 